MAKE A MEME View Large Image Nanoindent.JPG An AFM image of the residual indent left by a Berkovitch tip during a nanoindentation experiment on a Zr-Cu-Al metallic glass Image by Jonathan Puthoff University of Wisconsin - Madison en wikipedia 2007-01-08 Jputhoff ...
View Original:Nanoindent.JPG (779x722)
Download: Original    Medium    Small Thumb
Courtesy of:commons.wikimedia.org More Like This
Keywords: Nanoindent.JPG An AFM image of the residual indent left by a Berkovitch tip during a nanoindentation experiment on a Zr-Cu-Al metallic glass Image by Jonathan Puthoff University of Wisconsin - Madison en wikipedia 2007-01-08 Jputhoff wikipedia en Jputhoff original upload log page en wikipedia Nanoindent JPG 2007-01-08 20 44 Jputhoff 1016×722× 102973 bytes <nowiki>An AFM image of the residual indent left by a Berkovitch tip during a nanoindentation experiment on a Zr-Cu-Al metallic glass Image by Jonathan Puthoff University of Wisconsin - Madison </nowiki> Hardness tests